1. … of the weld deposit will degrees 16% at 300°C and about 30% at 600°C. The weld deposit is high heat resistant up to 900°C. DUR 6 …
  2. … oxidation, at service temperatures ranging from 1200°F (650°C) up to 1600°F (870°C) … AMS 5708, 5709, 5706, 5707, 5704, 5544, 5586. PWA 1005, …
  3. … alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. … Aircraft gas …
  4. … The 9%Cr-1%Mo creep resistant alloy is used for service up to ~600°C particularly in environments involving hot hydrogen gas. Flux …
  5. … of new, innovative welding processes and procedures. The location (600 m2) accommodates the highest quality and innovative welding …
  6. … of the weld deposit will degrease 16% at 300°C and about 30% at 600°C. Excellent alloy against thermal shock, abrasion, erosion, …
  7. … and by grinding. The hardness of the weld deposit will degreas 20% at 600°C and has a nominal hardness of 47-52 HRc at room temperature. The …
  8. … welding wires that are covered in AWS A 5.14 such as alloy 82, Inconel 600, 625, 601, 825, C276, alloy 59 etc. Basicity: about 3,3 (according … welding wires that are covered in AWS A 5.14 such as alloy 82, Inconel 600, 625, 601, 825, C276, alloy 59 etc. … FL 839 … 14174: SA FB 2 DC …
  9. … developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good resistance to general …
  10. … of the weld deposit will degrees 16% at 300 °C and about 30% at 600 °C. The weld deposit is high heat resistant up to 900 °C.  … …