1. … Replaceable polyurethane tyres are mounted onto a cast steel drumdor durability and siperior traction. … Euroweld - RedRock Column & Boom …
  2. … helium are used as shielding gases in TIG welding to prevent oxidation during the welding process. A well-maintained and properly adjusted …
  3. … from porosity due to the special shaving process and cleaning method during production. AlMg4,5Mn is one of the highest grades within the …
  4. … root of the weld on the first pass and blankets the solidified weld during subsequent passes until the root surface temperature stays below …
  5. … Weldable without protective gas.Corresponding electrode: CEWELD® Dur 62 S … 61-64 HRc hardfacing alloy, Cement, Mineral mixing, hammers, …
  6. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Grey Cast Iron, …
  7. … less than 1% nickel to full fill NACE requirements and cover more procedures up to 500 MPa yield strength steels. CEWELD® AA M500 can also be … 65, Oceanfit 355, Oceanfit 420, Oceanfit 460, alform plate 460M; durostat 400, 450, 500, durostat B2     … AA M500 … A 5.28: E80C-Ni1 H4 … A 5.36: …
  8. … to the extreme high hardness, please consult us for a succesfull procedure.  … Hardfacing Ni-hard in the cement industry …
  9. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast …
  10. … of the year 2015 in the district called "The Betuwe". It all happened during a exiting campaign evening of "Betuwe onderneemt Beter", Monday …