1. … a homogeneous weld and preserving the desired properties. CEWELD NiCro 718 filler materials are specifically designed to ensure …
  2. … hardness of the deposit will degrease 16% at 300°C and about 30% at 600°C. Excellent alloy against thermal shock, abrasion, erosion, …
  3. … welding in all positions. Excellent for use on ceramic backing strips. The slag is self detaching and offers extra protection to … CrNiMo 17 12 2, G-X 6 CrNiMo 18 10,         X 5 CrNiMo 17 13 3 UNS S31600, S31603, S31635, S31640, S31653,  AISI 316, 316L, 316Ti, 316Cb  … …
  4. … The 9%Cr-1%Mo creep resistant alloy is used for service up to ~600°C particularly in environments involving hot hydrogen gas. Flux …
  5. … 279°C / Deposit color: Silver / Shear Strength (copper lap joint): 10,600 PSI … Copper, stainless steel … S-SnAg5 …
  6. … of the weld deposit will degrease 16% at 300°C and about 30% at 600°C. Excellent alloy against thermal shock, abrasion, erosion, …
  7. … abrasion resistance can be kept up to working temperatures of 600 ºC ; the hardness is still 40-45 HRc at these temperatures. For …
  8. … for creep resistant service for working temperatures up to 600 ºC.  … 2,25% Cr, 1% Mo  1.7015, 1.7131, 1.7147, 1.7380, 1.7337, …
  9. … developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good resistance to general …
  10. … and by grinding. The hardness of the weld deposit will degrees 20% at 600 °C and has a nominal hardness of 49-53 HRc at room temperature. The …