1. … Replaceable polyurethane tyres are mounted onto a cast steel drumdor durability and siperior traction. … Euroweld - RedRock Column & Boom …
  2. … helium are used as shielding gases in TIG welding to prevent oxidation during the welding process. A well-maintained and properly adjusted …
  3. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Grey Cast Iron, …
  4. … Ti the weld deposit has much higher temperature scale-resistance up to 800 °C due to the increased silicon content. … ISO 15608: 8.1  Austenit …
  5. … old layers. Weldable without protective gas.Corresponding electrode: Dur 62 S … 64-68 HRc hardfacing alloy, Cement, Mineral mixing, hammers, …
  6. … third parties that enables you to use only one wire to cover more procedures up to 460 MPa yield strength steels. CEWELD AA M460 can also be …
  7. … range that anables you to use only one wire to cover more procedures upto 620N/mm2 yield strenght steels. AA M610 can also be used for … Domex 600 MC, Domex 650 MC, Domex 600 MC, Hardox 400, XAR 400, Dillidur 400, Oceanfit 100, Oceanfit 600, alform plate 620 M,  aldur 620 Q, 620 QL, 620 QL1,    … AA M610 … A 5.28: E100C-K3 H4 … …
  8. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast …
  9. … The weld deposit is scale-resistant up to approx. 800 °C in normal atmosphere and oxidizing gases. The weld deposit is …
  10. … in case of old layers or critical base metals. Equivalent in SMAW: Dur 64 … For fire gratings, sintering plants, augers and blast furnace …